90W10Cu tungsten copper properties are:
At 950 ℃ high speed pressing attainable relative density greater than 80.65% of W
skeleton, by infiltration get 90W10Cu composites.
At room temperature, 600 ℃, 950 ℃ for high-speed tungsten preform pressing, pressing as the temperature rises, the green density increases.
At room temperature, 600 ℃, 950 ℃ for high-speed tungsten preform pressing, pressing as the temperature rises, the green density increases.
High velocity compaction, powder mass increases, due to the ability of
additional density decreases, resulting green density decreases. With the increase
in the number of high-speed pressing, green density is improved.
Using high-speed pressing technology combined with infiltration of 90W10Cu preparation material and the thermal expansion coefficient and other indicators have reached the requirements of the appropriate heat sink material.
If
you have any inquiry of tungsten copper, please feel free to contact
us:
Tel.:
+86 592 5129696/+86 592 5129595
Fax:
+86 592 5129797
Scan
QR code of Chinatungsten Wechat platform to follow up the daily latest price
and market of tungsten, molybdenum and rare earth.
没有评论:
发表评论